Sanmac® 2205

Hollow barDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanmac® 2205 is a duplex (austenitic-ferritic) stainless steel with improved machinability. The grade is characterized by:

  • Excellent machinability
  • High resistance to stress corrosion cracking (SCC) in chloride-bearing environments
  • High resistance to stress corrosion cracking (SCC) in environments containing hydrogen sulfide
  • High resistance to general corrosion, pitting and crevice corrosion
  • High mechanical strength – roughly twice the proof strength of austenitic stainless steels
  • Good hot-working properties
  • High resistance to erosion corrosion and corrosion fatigue
  • Physical properties that offer design advantages
  • Good weldability

Standards

  • UNS: S31803, S32205
  • EN Number: 1.4462
  • EN Name: X2CrNiMoN22-5-3

Product standards
EN 10216-5, EN 10297-2, EN 10294-2

ASTM A790

Approvals

  • Approved by the American Society of Mechanical Engineers (ASME) for use in accordance with ASME Boiler and Pressure Vessel Code, section VIII, div. 1 and section VIII, div. 2, Case 2067-2
  • NACE MR 0175 (sulfide stress cracking resistant material for oil field equipment)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.