Sanmac® 4305

Hollow barDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanmac® 4305 is an austenitic chromium-nickel steel with extremely high machinability. For example, cutting speeds of up to twice those for Sanmac 304/304L can be used.

Standards

  • ASTM: MT 303
  • UNS: S30300
  • EN Number: 1.4305

Product standards

  • EN 10297-2, EN 10294-2
  • ASTM A511

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.