Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanmac® 4571 is titanium-stabilized austenitic stainless chromium–nickel–molybdenum steel with improved machinability.

Standards

  • ASTM: 316 Ti
  • UNS: S31635
  • EN Number: 1.4571
  • EN Name: X6CrNiMo17-12-2

Product standards

Hollow Bar:

  • EN 10216-5*, EN 10294-2, EN 10297-2
  • ASTM A312, (ASTM A511)

* The leakage test is deferred to the finished component

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.