Sanbar® 20

Hollow drill steelDatasheet

Datasheet updated 2021-10-29 11:48 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanbar® 20 is a high-strength chromium-molybdenum steel with high fatigue strength and excellent wear resistance in the as-rolled condition.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.