Sanicro® 28 is a multi-purpose austenitic stainless ELC alloy for service in highly corrosive conditions. It is characterized by:

  • Very high corrosion resistance in strong acids
  • Very good resistance to stress and intergranular corrosion in various environments
  • Very high resistance to pitting and crevice corrosion
  • Good weldability

Standards

  • UNS: N08028
  • EN Number: 1.4563
  • EN Name: X 1 NiCrMoCu 31-27-4
  • W.Nr.: 1.4563
  • SS: 2584

Product standards

EN 10088-3

Certificates

Status according to EN 10 204 3.1

Chemical composition (nominal) %

C Si Mn P S Cr Ni Mo Cu
≤0.020 ≤0.6 ≤2.0 ≤0.025 ≤0.010 26.5 30.5 3.3 1.0

Forms of supply

Sizes and tolerances

Round-cornered square, as well as round billets, are produced in a wide range of sizes according to the following tables. Larger sizes offered on request.

Surface conditions

Square billets

Unground, spot ground or fully ground condition.

Round billets

Peel turned or black condition.

Square billets
Size
mm
Tolerance
mm
Length
m
80 +/-2 4 - 6.3
100, 114, 126, 140, 150 +/-3 4 - 6.3
160, 180, 195, 200 +/-4 4 - 6.3
>200 - 350 +/-5 3 - 5.3

Sizes and tolerances apply to the rolled/forged condition.

Peel turned round billets
Size
mm
Tolerance
mm
Length
m
75 - 200 (5 mm interval) +/-1 max 10
>200 - 450 +/-3 3 - 8
Unground round billets
Size
mm
Tolerance
mm
Length
m
77 - 112 (5 mm interval) +/-2 max 10
124, 134 +/-2 max 10
127, 147, 157 +/-2 max 10
142, 152, 163 +/-2 max 10
168, 178, 188 +/-2 max 10
183, 193 +/-2 max 10

Other products

Seamless tube and pipe
Hollow bar

Mechanical properties

Sanicro® 28 conforms to the mechanical properties according to specification EN 10088-3.

Testing is performed on separately solution annealed and quenched test pieces.

At 20°C (68°F)

Metric units
Proof strength Tensile strength Elong. HB
Rp0.2a) Rm Ab)
MPa MPa %
≥220 500-750c) ≥35 ≤220
Imperial units
Proof strength Tensile strength Elong. Hardness
Rp0.2a) Rm Ab) Rockwell C
ksi ksi %
approx.
≥32 72-108 ≥35 14

1 MPa = 1 N/mm2
a) Rp0.2 corresponds to 0.2% offset yield strength.
b) Based on L0 = 5.65√S0 , where L0 is the original gauge length and S0 the original cross-sectional area.

Impact strength

Due to its austenitic microstructure, Sanicro® 28 has very good impact strength, both at room temperature and at cryogenic temperatures.

Tests on bar have demonstrated that the steel fulfils the requirements according to the European standards EN13445-2(UFPV-2)(min.60J(44ft-lb)at-270oC(-455oF))andEN10272(min.60J(44ft-lb)at-196oC.(-320oF).


Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Alleima materials.