APM 2327, UNS S32505

Hot isostatic pressed (HIP) productsDatový list

Datový list byl aktualizován2019-12-17 08:00 (nahrazuje všechna předchozí vydání)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

APM 2327 is a powder metallurgical super duplex stainless steel. Compared to conventional duplex steels the grade has improved mechanical properties, corrosion resistance and superior corrosion fatigue performance.

The chemical composition is optimized for manufacturing large components with high wall thickness and is very similar to ASTM A182-F61 (UNS S32550) which requires max. 0.25% nitrogen. The corresponding European norm, W.Nr 1.4507, allows 0.30% nitrogen. APM 2327 has a nitrogen content of 0.25-0.30% which gives improved corrosion and mechanical properties.

Standards

  • ASTM: A988
  • UNS: S32505
  • EN Number: 1.4410

Approvals

  • Qualified according to NORSOK M650 (D52 eller D54). Maximum thickness 200 mm

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.