Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

APM 2377 is a powder metallurgical duplex (austenitic-ferritic) stainless steel manufactured by Hot Isostatic Pressing (HIP). It is characterized by high strength and good corrosion resistance. Applications include for example offshore components.

Standards

  • UNS: S31803, S32205
  • EN Number: 1.4462

Approvals

  • NACE MR0175/ISO 15156
  • ASME B31.3
  • APM 2377 supplied by Sandvik is qualified according to NORSOK M650 D44

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.