Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 20C is a hardened and tempered carbon steel characterized by:

  • High strength
  • High fatigue strength under bending and impact stress
  • Low level of non-metallic inclusions
  • Good wear resistance

Compressor valve steel in Sandvik 20C has excellent surface finish, good dimensional tolerances and good flatness.

Standards

  • ASTM: 1095
  • W.Nr.: 1.1274
  • SS: 1870

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via email