Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik Hiflex® is a hardened and tempered martensitic stainless compressor valve steel alloyed with molybdenum. The material is characterized by:

  • High strength and good ductility
  • Extremely high fatigue strength under bending and impact stress
  • Excellent surface finish
  • Very high compressive residual surface stress
  • Low level of non-metallic inclusions
  • Good wear resistance

Sandvik Hiflex® compressor valve steel has good dimensional tolerances and good flatness.

Standards

  • UNS: S42026
  • EN Number: (1.4031)*

*) Nearest equivalent grade

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.