Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

SAF 2507® is a super-duplex (austenitic-ferritic) stainless steel for service in highly corrosive conditions. The grade is characterized by:

  • Excellent resistance to stress corrosion cracking (SCC) in chloride-bearing environments
  • Excellent resistance to pitting and crevice corrosion
  • High resistance to general corrosion
  • Very high mechanical strength
  • Physical properties that offer design advantages
  • High resistance to erosion corrosion and corrosion fatigue
  • Good weldability

Standards

  • UNS: S32750
  • EN Number: 1.4410
  • EN Name: X 2 CrNiMoN 25-7-4
  • SS: 2328

Product standards

  • Seamless tube and pipe: EN 10216-5
  • Seamless and welded tube and pipe: ASTM A789; A790
  • Flanges: ASTM A182
  • Fittings: ASTM A182; (ASTM A815 applied for)
  • Plate, sheet and strip: ASTM A240, EN 10088-2
  • Bar steel: ASTM A479, EN 10088-3
  • Forged billets: EN 10088-3 

Approvals

  • Approved by the American Society of Mechanical Engineers (ASME) for use in accordance with ASME Boiler and Pressure Vessel Code, Section VIII, div. 1. There is no approval for UNS S32750 in the form of plate. However, according to ASME paragraph UG-15, the design values for seamless tube according to ASME Section VIII, div. 1 are also allowed to be used for plate.
  • ASME B31.3 Chemical Plant and Petroleum Refinery piping
  • VdTÜV-Werkstoffblatt 508
  • NACE MR0175/ISO 15156 (Petroleum and natural gas industries - Materials for use in H2S-containing Environments in oil and gas production - Part 3: Cracking-resistant CRAs (corrosion resistant alloys and other alloys) (Published:2015)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.