Sandvik 2RE10

Tube and pipe, seamlessDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 2RE10 is an austenitic stainless steel with extremely low carbon and impurity contents. The grade is characterized by:

  • Excellent resistance to corrosion in nitric acid
  • Excellent resistance to intergranular corrosion
  • Good resistance to pitting
  • Good weldability

Standards

  • UNS: S31002
  • EN Number: 1.4335
  • W.Nr.: 1.4335*
  • DIN: X 1 CrNi 25 21*

* Obsolete. Replaced by EN.

Product standards

  • ASTM A213 and A312
  • EN 10216-5
  • SEW 400 (Feb 1991)

Sandvik 2RE10 conforms to EN no. 1.4335, but actual composition specified for EN no. 1.4335 allows considerable higher maximum levels of C, Si, P, S and Mo. High levels of these elements increase the potential for corrosion and have therefore been kept as low as possible in Sandvik 2RE10.

Approvals

  • ASME Code Case 2591. Section VIII, Division 1.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.