Sandvik 3R19

Tube and pipe, seamlessDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 3R19 is an austenitic stainless steel with low carbon content alloyed with nitrogen.

Standards

  • ASTM: TP304LN
  • UNS: S30453
  • EN Number: 1.4311
  • W.Nr.: 1.4311*
  • DIN: X 2 CrNiN 18 10*
  • SS: 2371*
  • AFNOR: Z2CN18-10Az*

* Obsolete. Replaced by EN.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.