Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.

Sandvik 3R65 is a molybdenum-alloyed austenitic stainless chromium-nickel steel with a low carbon content. The grade is characterized by:

  • Good resistance to general corrosion and better resistance to pitting than ASTM TP304, because of the alloying with molybdenum (Mo).
  • High tensile strength

Sandvik 3R65 is used for medical tools.

Standards

  • ASTM: TP316L, TP316
  • UNS: S31603, S31600
  • EN Number: 1.4404, 1.4401
  • EN Name: X2CrNiMo17-12-2, X5CrNiMo17-12-2
  • W.Nr.: 1.4404, 1.4401
  • DIN: X 2 CrNiMo 17 13 2, X 5 CrNiMo 17 12 2
  • SS: 2348
  • AFNOR: Z 2 CND 17.12, Z 6 CND 17.11
  • BS: 316S11

Product standards

  • ASTM F899, A213, A269, A312
  • ISO 16061
  • EN 10216-5
  • BS 3605, BS 3606
  • DIN 17456, 17458
  • NFA 49-117, 49-217
  • SS 14 23 48

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.