Sandvik 3R65

Tube and pipe, seamlessDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 3R65 is a molybdenum-alloyed austenitic stainless chromium-nickel steel with a low carbon content.

Standards

  • ASTM: TP316L, TP316
  • UNS: S31603, S31600
  • EN Number: 1.4404, 1.4401
  • EN Name: X2CrNiMo17-12-2, X5CrNiMo17-12-2
  • W.Nr.: 1.4404, 1.4401
  • DIN: X 2 CrNiMo 17 13 2, X 5 CrNiMo 17 12 2
  • SS: 2348
  • AFNOR: Z 2 CND 17.12, Z 6 CND 17.11
  • BS: 316S11

Product standards

  • ASTM A213, A269, A312
  • EN 10216-5
  • BS 3605, BS 3606
  • DIN 17456, 17458
  • NFA 49-117, 49-217
  • SS 14 23 48

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.