Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 4C54 is a ferritic, heat resisting, stainless chromium steel, characterized by:

  • Extremely good resistance to reducing sulphurous gases
  • Very good resistance to oxidation in air
  • Good resistance to oil-ash corrosion
  • Good resistance to molten copper, lead and tin

This steel can be used at temperatures up to 1100°C (2010°F). However, allowance should be made for low creep strength at the highest temperatures in order to avoid distortion due to the mass of the steel.

Standards

  • ASTM: 446-1
  • UNS: S44600
  • EN Number: 1.4749
  • W.Nr.: 1.4749
  • DIN: X 18 CrN 28
  • SS: 2322

Product standards

  • ASTM A268
  • EN 10297-2
  • SS 14 23 22

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.