Sandvik Formula 1

Weld finishing Datový list

Datový list byl aktualizován 2018-07-25 11:05 (nahrazuje všechna předchozí vydání)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik Formula 1 is an effective multipurpose pickling paste used for post-weld treatment of stainless steel welds. Stainless steels are pickled in order to refurbish the welds surface finish by removing welding oxide, heat tint or scale, formed during fabrication. Sandvik Formula 1 effectively removes these oxides and the chromium depleted area that will reduce the corrosion resistance of the stainless steel surface.

Sandvik Formula 1 is rapid and economical to use, as only a thin film of the pickling paste is required for a perfect result. The pickling paste has excellent adhesion and can be applied on vertical surfaces and ceilings without any risk of running or drying.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.