Exaton 42

Welding wire Datový list

Datový list byl aktualizován 2017-10-26 10:04 (nahrazuje všechna předchozí vydání)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Exaton 42 is a duplex stainless steel of type UNS S32760 for use in aggressive environments where high mechanical strength and high corrosion resistance is required.

Compared to Sandvik 25.10.4.L the filler is alloyed with Cu and W which makes it somewhat more prone to intermetallic phases.

Standards

  • ISO 14343: 25 9 4 N L
  • AWS A5.9/ASME SFA-5.9: ER2594
  • W.Nr.: (1.4501)*

* nearest equivalent

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.