Sandvik 19.9.NbSi

Welding wire Datový list

Datový list byl aktualizován 2019-07-12 14:27 (nahrazuje všechna předchozí vydání)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 19.9.NbSi is a filler metal mainly suited for MIG welding of stainless steels of the 18Cr/8Ni/Nb and 18Cr/8Ni/Ti types.

Standards

  • ISO 14343: 19 9 Nb Si
  • AWS A5.9/ASME SFA-5.9: ER347Si
  • W.Nr.: 1.4551

Product Approvals

  • CE
  • DB
  • TÜV

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.