Exera® Finemac™ free-cutting wire

WireDatasheet

Datasheet updated 2021-02-02 16:09 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Exera® Finemac™ is a lead-free, hardenable, free-cutting carbon steel characterized by excellent machinability and high hardness, high wear resistance and exceptional dimensional stability after hardening.

Hardening operations are very much simplified compared to Sandvik 20AP, owing to the wider temperature and time range available using Exera® Finemac™. This results in significantly reduced failure rates during hardening. Exera® Finemac™ also exhibits very good cold heading properties. The material is suitable for long, narrow components with tight tolerances.

Service temperature -50 to 100°C (-55 to 210oF). Prolonged service at elevated temperatures causes decreased hardness when used in the hardened and tempered condition.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.