Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.

Exera® High-N is a molybdenum and nitrogen alloyed austenitic stainless steel, used for orthopedic implants and fracture fixation devices.

The grade is characterized by:

  • Proof strength is up to twice that of Exera® 316LVM in the annealed condition
  • Higher corrosion resistance than Exera® 316LVM
  • High microcleanliness
  • Very good surface finish
  • Good forgeability

Standards

  • UNS: S31675
  • BS: 7252-9

Product standard

  • ASTM F1586

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.