Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 11R51® is an austenitic stainless steel alloyed with molybdenum. The grade is characterized by high tensile strength and high resistance to corrosion, fatigue and relaxation.

Compared to most other steels of ASTM 302 type (for example Sandvik 12R10/gusab T302), Sandvik 11R51® offers:

  • Higher tensile strength and tempering effect
  • Higher relaxation resistance, especially at elevated temperatures
  • Higher fatigue strength
  • Better corrosion resistance, through the addition of molybdenum

Service temperature: -200 to 300°C (-330 to 570°F).

Standards

  • UNS: S30151
  • ISO: X9 CrNi 18-8
  • EN Number: 1.4310
  • EN Name: X10 CrNi 18-8

Product standards

EN 10270-3
ISO 6931-1
ASTM A 313/A 313M

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.