Sandvik Springflex™ SH spring wire

Wire Datový list

Datový list byl aktualizován 2018-07-18 16:04 (nahrazuje všechna předchozí vydání)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik Springflex™ SH is a duplex (austenitic-ferritic) stainless steel characterized by:

  • Extremely high tensile strength in 'as delivered' condition
  • Very good relaxation resistance
  • High resistance to stress corrosion cracking (SCC) in chloride-bearing environments
  • High resistance to stress corrosion cracking (SCC) in environments containing hydrogen sulphide
  • High resistance to general corrosion, pitting, and crevice corrosion
  • High resistance to erosion corrosion and corrosion fatigue
  • Physical properties that offer design advantages

Service temperature: -100 to 300°C (-150 to 570°F)

Standards

  • UNS: S32205/S31803
  • EN Number: 1.4462
  • EN Name: X2CrNiMoN 22-5-3

Product standard

  • EN 10270-3 is valid, excluding chemical composition and mechanical properties.
  • ASTM A313

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.