Sanicro® 26Mo for wirelines

Wire Datový list

Datový list byl aktualizován 2018-07-18 15:49 (nahrazuje všechna předchozí vydání)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 26Mo is a high-alloy austenitic stainless steel for service in highly corrosive conditions in oil and gas environments. The grade is characterized by:

  • Very good resistance to stress corrosion cracking (SCC) in H2S, chloride and CO2 environments
  • Very good resistance to pitting in chloride-containing environments because of its high PRE* value of 43 minimum
  • Very good resistance to general corrosion
  • High mechanical strength and correspondingly high breaking loads
  • Maximum recommended service temperature: 250°C

* PRE, Pitting Resistance Equivalent = %Cr + 3.3 x %Mo + 16 x %N

Standards

  • UNS: N08926
  • W.Nr.: 1.4529

Standards

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.