Austenitic stainless steel metal powder

Sandvik's standard range of Osprey™ austenitic stainless steel metal powder includes grades of ASTM 304L, 310S and 316L types. This powder is used in processes, such as:

Chcete vědět víc?

Zavolejte nám Zašlete nám e-mail

General grades

General austenitic stainless steel grades

Selected austenitic stainless steels incl. chemical composition (nominal), %
Alloy (UNS)DescriptionFeCCrNiMoSiMnSP
304L
(S30403)
See below1) Bal. 0.03 18.0-
20.0
8.0-
12.0
- 1.0 2.0 0.03 0.045
310S
(S31008)
See below2) Bal. 0.08 24.0-
26.0
19.0-
22.0
- 1.5 2.0 0.03 0.045
316L
(S31603)
See below3) Bal. 0.03 16.0-
18.0
10.0-
14.0
2.0-
3.0
1.0 2.0 0.03 0.045
'904L' See below4) Bal. 0.02 19.0-23.0 23.0-28.0 4.0-5.0 1.0 2.0 0.035 0.045

1) Essentially non-magnetic, becomes slightly magnetic when cold worked. Low carbon content means less carbide precipitation in the heat-affected zone during welding and a lower susceptibility to intergranular corrosion.
2) Low carbon type 310 – for welding.
3) Good corrosion resistance to most chemicals. High creep strength at elevated temperatures. The low carbon content redices the possibility of in vivo corrosion for medical applications.
4) High-alloy austenitic stainless steel characterized by very good resistance to general corrosion in sulphuric, phosphoric and acetic acid as well as very good resistance to pitting corrosion and stress corrosion cracking.

Other austenitic stainless steels are also available. Contact us to discuss Sandvik's full range of metal powder alloys.

Thermal spray alloys

Austenitic stainless steel grades for thermal spray

Selected austenitic stainless steels for thermal spray, including flame spray and metallizing incl. chemical composition (nominal), %
Alloy Description Fe C Cr Si Mn Ni Others
SC 30 Austenitic stainless steel of 304 type Bal. 0.08 19.0 1.0 2.0 10.0 -
SC 304L Low-carbon austenitic stainless steel Bal. 0.02 19.0 1.0 2.0 10.0 -
SC 316L Corrosion resistant stainless steel Bal. 0.02 17.0 1.0 2.0 12.0 Mo 2.5

Other austenitic stainless steels are also available. Contact us to discuss Sandvik's full range of metal powder alloys.