MCrAlY alloy metal powder

Sandvik's standard range of Osprey™ metal powders includes MCrAlY alloys used for plasma and thermal spray.

Chcete vědět víc?

Zavolejte nám Zašlete nám e-mail

Selected MCrAlY alloys incl. chemical composition (nominal), %
Alloy Fe Cr Ni Co C Mn Si Y Al
FeCrAlY Bal. 10–30 0-5 - 0.1 0.5 0.2 1 5–30
NiCrAlY - 20–30 Bal. - 0.1 0.5 0.2 1 0–10
CrCrAlY - 20–35 - Bal. 0.1 0.5 0.2 1 0–10
CoNiCrAlY - 25–35 15–25 Bal. 0.1 0.5 0.2 1 0–10
CrAlY - Bal. - - 0.1 0.5 0.2 2 20–30

Other MCrAlY alloys are also available. Contact us to discuss Sandvik's full range of metal powder alloys.