Compressor valve steel grades
Our program of hardened and tempered compressor valve steel includes two types of stainless steel and one carbon steel.
grade | Description |
---|---|
FreeflexTM | A hardened and tempered martensitic stainless compressor valve steel alloyed with copper with excellent dimensional tolerances and flatness. |
Hiflex™ | A new generation of high-fatigue resistance stainless chromium steel giving design freedom for valves in high-frequency and high-pressure compressors. |
7C27Mo2 | A martensitic stainless chromium steel alloyed with molybdenum that has higher fatigue strength than our 20C. |
20C* | A carbon steel with 1% carbon, offering high fatigue strength. |
Our grade | Tensile strength, MPa (ksi) | Thickness, mm (in.) |
---|---|---|
FreeflexTM | 2020 (293) | 0.076-0.6 (0.003-0.0236) |
Hiflex™ | 1900 (276) | 0.152-1.0 (0.006-0.026) |
7C27Mo2 | 1800 (261) | 0.152-1.2 (0.006-0.047) |
20C* | 1600-2100 (232-305) | 0.152-1.2 (0.006-0.047) |
* Contact us for more information