Sandvik 12C27M knife steel

Dishwasher safe

Sandvik 12C27M knife steel was developed for highest possible edge performance while still having good enough corrosion resistance for daily use in a dishwasher.

Chcete vědět víc?

Zavolejte nám Zašlete nám e-mail

Buy samples of Sandvik 14C28N knife steel

Now in stock, so don't miss this opportunity!

Current availability:

  • USA & Canada: Hobbyists / consumers over 18 years of age and business customers
  • European Union: Hobbyists / consumers over 18 years of age and business customers
  • Rest of the world: Business customers only

Buy sample


Sandvik 12C27M knife steel is a step up in corrosion resistance from Sandvik 12C27 and the number one choice for edge applications where increased corrosion resistance is important together with high demands on edge performance and toughness.

With a hardness range of 53-59 HRC, excellent toughness and great corrosion resistance this knife steel grade is the recommended choice for kitchen knives, high-end scissors, gardening tools, professional butcher knives and fishing knives for fresh water environments.

Like most of Sandvik's knife steels this grade is fineblankable enabling efficient production.

Chemical composition, % (nominal)
Carbon
(C)
Chromium
(Cr)
Molybdenum
(Mo)
Silicon
(Si)
Manganese
(Mn)
0.52 14.5 - 0.40 0.60

Datasheet

Sandvik 12C27M