Sandvik 13C26 knife steel

Razor edge sharpness

Sandvik 13C26 knife steel is developed for razor blade applications which means a strong focus on hardness, sharpness and edge stability.

Chcete vědět víc?

Zavolejte nám Zašlete nám e-mail

Buy samples of Sandvik 14C28N knife steel

Now in stock, so don't miss this opportunity!

Current availability:

  • USA & Canada: Hobbyists / consumers over 18 years of age and business customers
  • European Union: Hobbyists / consumers over 18 years of age and business customers
  • Rest of the world: Business customers only

Buy sample


Sandvik 13C26 is the Sandvik knife steel grade with the highest achievable hardness while still maintaining the fine carbide structure which is characteristic for Sandvik's knife steels.

With exceptional edge performance and good toughness this grade is an excellent choice for demanding cutting applications where the moderate corrosion resistance of Sandvik 13C26 knife steel is not a key issue, or if the blade is coated for corrosion protection.

With a recommended hardness range of 55-62 HRC, exceptional edge performance with scary sharpness and good toughness, Sandvik 13C26 knife steel is recommended for surgical blades, razor applications, whittling or as a surface coated EDC (Every Day Carry) knife.

Like most of Sandvik's knife steels this grade is fineblankable enabling efficient production.

Chemical composition, % (nominal)
Carbon
(C)
Chromium
(Cr)
Molybdenum
(Mo)
Silicon
(Si)
Manganese
(Mn)
0.68 12.9 - 0.40 0.60

Datasheet

Sandvik 13C26