Sandvik 7C27Mo2 knife steel

High corrosion resistance

Sandvik 7C27Mo2 is Sandvik's most corrosion-resistant knife steel. It combines exceptional corrosion resistance with decent edge properties.

Chcete vědět víc?

Zavolejte nám Zašlete nám e-mail

Buy samples of Sandvik 14C28N knife steel

Now in stock, so don't miss this opportunity!

Current availability:

  • USA & Canada: Hobbyists / consumers over 18 years of age and business customers
  • European Union: Hobbyists / consumers over 18 years of age and business customers
  • Rest of the world: Business customers only

Buy sample


The main reason for choosing this grade over other Sandvik knife steels is the benefits of high corrosion resistance, toughness and ease of re-sharpening. The added corrosion resistance is beneficial, especially when pitting corrosion is the main reason for the deterioration of the knife edge.

With a hardness range of 53-57 HRC Sandvik 7C27Mo2 is recommended for fishing knives and outdoor knives used in marine environments.

Like most of Sandvik's knife steels this grade is fineblankable enabling efficient production.

Carbon
(C)
Chromium
(Cr)
Molybdenum
(Mo)
Silicon
(Si)
Manganese
(Mn)
0.38 13.5 1 0.40 0.55

Datasheet