Size range for Sandvik knife steel

The table shows the size range for Sandvik knife steels. Sandvik knife steel is delivered in coils or as straightened lengths.

Chcete vědět víc?

Zavolejte nám Zašlete nám e-mail

Sandvik grade Width, mm (in.) Thickness, mm (in.)
Size range for Sandvik knife steels
Sandvik 6C27 5 - 380
(0.1968 - 14.96)
0.1 - 2.5
(0.004 - 0.098)
Sandvik 7C27Mo2 5 - 350
(0.1968 - 13.78)
0.1 - 4.5
(0.004 - 0.177)
Sandvik 12C27 10 - 380
(0.394 - 14.96)
1.00 - 4.5
(0.04 - 0.177)
Sandvik 12C27M 10 - 380
(0.394 - 14.96)
1.00 - 4.5
(0.04 - 0.177)
Sandvik 13C26 5 - 380
(0.1968 - 14.96)
0.1 - 3.0
(0.004 - 0.118)
Sandvik 14C28N 5 - 380
(0.1968 - 14.96)
1.00 - 4.5
(0.04 - 0.177)
Sandvik 19C27 5 - 340
(0.1968 - 13.38)
0.1 - 3.0
(0.004 - 0.118)

Hardening guide