Sandvik SAF 3207, also known as Sandvik SAF 3207 HD, is Sandvik's trademark for a hyper-duplex stainless steel developed for deep-water umbilicals. The grade is characterized by excellent resistance to stress corrosion cracking (SCC), pitting and crevice corrosion, high resistance to general corrosion and excellent mechanical strength.