Finned and smooth ethylene furnace tubes

Ethylene furnace tubes in Sandvik 353 MA*, a material characterized by high creep strength and high resistance against carburization. Combined with very good oxidation properties at high temperatures, the use of Sandvik 353 MA tubes can contribute to longer production runs before decoking.
Sandvik ethylene furnace tubes are supplied in a wrought condition and with a smooth or finned design, both bringing efficiency benefits when used for steam cracking furnace tubes in ethylene production.
100% ultrasonic test
All Sandvik ethylene furnace tubes are 100% ultrasonically tested to ensure that they are free from defects such as micro cracks, which significantly contributes to reduced decoking rate.