Laying head pipe

Sandvik SAF 2507 LHP for laying head pipe is a high alloy super-duplex stainless steel.

Chcete vědět víc?

Zavolejte nám Zašlete nám e-mail

Main characteristics of Sandvik SAF 2507 LHP

  • Very high mechanical strength
  • Excellent wear resistance at high temperatures

Thermal expansion

Sandvik SAF 2507 LHP has a coefficient of thermal expansion close to that of carbon steel. This gives Sandvik SAF 2507 LHP definite design advantages over austenitic stainless steels in equipment comprising both carbon steel and stainless steel. The values given below are average values in the temperature ranges.

Metric units x10-6/°C

Temperature, °C 30-100 30-200 30-300 30-400
Sandvik SAF 2507 LHP 13.5 14.0 14.0 14.5
Carbon steel 12.5 13.0 13.5 14.0
ASTM 316L 16.5 17.0 17.5 18.0

Figure 1. Thermal expansion comparison between grades.

Modern mills

Historic development

  • Rolling rods of OD 5,5 mm at speeds up to 150 m/s (this requires LHP with ID ≈ 20 mm)
  • LHP with reduced bore sized (ID ≈ 20 mm) should be used for small diameter products (OD = 4 ÷ 12 mm) for a more consistent pattern

Historic development of 5.5 mm wire rod rolling speed, mill capability (m/s)

Figure 2. Forced productivity, sub-optimization.

Common problems

  • Higher rolling speeds → acceleration of pipe wear
  • LHP wear → unstable laying ring pattern
  • Possibility of wire breaking in pipe ("cobble")
  • Wire rod produced with inconsistent mechanical properties and tolerances

Read more about wire rod rolling