Exera® Bondable Coatings
Bondable coatings can be applied to bare wire or as a second coat over the top of any of the insulations that are offered. The amount of coating applied can be standard NEMA or JIS build or thinner amounts as required.
If a special coating or insulation is required Sandvik will work with you to develop a process for its use. Sandvik has, for example, developed low out-gassing, high-temperature, self-bondable coatings specifically designed for the hard disk drive industry to reduce contamination and deliver good resonance performance.
Exera® designation | Description | Maximum usage temperature* | Bonding technique |
---|---|---|---|
Bond B | Thermoplastic polyvinyl butyral | 100°C (210°F) | Methanol, acetone or heat activated |
Bond CJL | Thermoplastic polyester | Acetone, methyl ethyl ketone or heat activated | |
Bond E1 | Thermoplastic epoxy | 130°C (265°F) | Acetone, MEK or heat activated |
Bond MA | Thermoplastic polyamide | 155°C (310°F) | Methyl alcohol, isopropyl alcohol or heat activated |
Bond TT | Thermoplastic polyamide | Isopropyl alcohol or heat activated | |
Bond XTS | Thermosetting epoxy | 155°C (310°F) | MEK or heat activated |
Bond XTC | Thermoplastic polyamide | 200°C (390°F) | Heat activated |
Bond MA50** | Thermoplastic polyamide | 200°C (390°F) | Methyl alcohol or heat activated |
Sulfones | |||
Tecothane |
* The maximum usage temperature is based on the temperature at which the adhesive retains 5 - 10% of it's room temperature strength.
** Contact us for more information.
Metallic coatings
Sandvik provides several types of metallic coatings such as anodizing, electroplating and electropolishing. As a standard, Sandvik offers gold-plated wire, nickel-plated wire and silver-plated wire, but also other types of electroplating can be manufactured on request. Additionally, Sandvik works with cladding and cladded alloys.