Caribbean plant extends tube life from two to 15 years with Sandvik hyper-duplex stainless steel

By replacing its existing heat exchanger tube with hyper-duplex stainless steel by Sandvik, a major Caribbean furfural producer has extended its tube lifecycles from two to 15 years.

Reducing heat exchanger shutdowns

By using tubes in SAF 2707 HD, a German oil refinery reduced the number of heat exchanger shutdowns from eight to one.

Resisting corrosion in sulphide-rich environment

Sanicro 28 tubes proved to be a safe choice to fight hydrogen induced cracking in the heat exchangers of a large Indian oil refinery.

Prolonging lance tube service life

Halved lance tube consumption and increased productivity with Sandvik 253 MA.