Borax

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Bromine

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Calcium sulphide

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Camphor

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Chloric acid

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Chloroform

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Chlorohydrin

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Chlorosulphonic acid

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Chlorotoluene

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Citric acid

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and