677 hits

677 hits on all pages in Materials center

Detergents

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Ethyl alcohol

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Ethylene bromide

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Fatty acids

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Fixing salt

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Oxidation

Oxidation is the reaction of metal and oxygen. If the oxide formed is continuous and effective in separating the alloy from the atmosphere, the oxide is protective. However, if the oxide fails to act as a separator, problems with corrosion occur.

Acetic acid

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Acetyl chloride

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Adipic acid

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Alum

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Go to page: Previous , 1 , , 61 , 62 , 63 , 64(This page) , 65 , 66 , 67 , 68 Next