Carbon disulphide

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Cellulose acetate

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Chloramine

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Chloride of lime

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Chlorine

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Chlorine dioxide

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Chloroacetic acid

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Copper cyanide

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Pitting corrosion

Pitting corrosion is a form of localized corrosion, which produces attacks in the form of spots or pits. Pitting corrosion may occur in stainless steels in neutral or acid solutions containing halides*, primarily chlorides (Cl - ), such as seawater.

Acetic acid + formic acid

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and