Standard:ASTM 420 | EN number 1.4028 Mod./1.4031 Mod.
A martensitic stainless chromium steel with very good formability that after hardening and tempering is characterized by high corrosion resistance and toughness. The grade is part of the Exera® medical materials range.
Vis datablad for:
UNS S30815 | ASTM F45 | EN number 1.4835
An austenitic chromium-nickel steel alloyed with nitrogen and rare earth metals for high-temperature applications. Sandvik 253 MA is characterized by high creep strength, very good resistance to isothermal and cyclic oxidation.
Adskillige tilgængelige produktformularer:
Standard:UNS S42026 | EN number 1.4034*
Sandvik Sanprint® RPS is a hardened and tempered chromium steel used for printing doctor blade applications. The grade is a standard martensitic stainless steel suitable for water-based inks and laminating.
Standard:UNS N07750
A precipitation hardening nickel alloy with good spring properties and good resistance to gas corrosion at high temperatures.
Standard:
A family of hardened and tempered martensitic chromium steels used for a wide range of precision components.
A martensitic stainless chromium steel which after hardening is characterized by very high hardness and wear resistance and good corrosion resistance. The grade is part of the Sandvik medical materials range.
Standard:UNS S45500
A precipitation hardening stainless steel. In the annealed condition the formability is good and by a simple heat treatment the material obtains extensive precipitation hardening.
A hardened and tempered carbon steel with moderate tensile strength.
Standard:UNS S35315 | EN number 1.4854
An austenitic chromium-nickel steel alloyed with nitrogen and rare earth metals for high-temperature applications. The grade is characterized by high creep strength, very good resistance to isothermal and cyclic oxidation as well as very good resistance to nitration and carburization.
Standard:EN number 1.4742**
A ferritic chromium steel for high-temperature applications. Sandvik 1C356 is characterized by very good resistance to reducing sulphurous gases and good resistance to oxidation in air and oxidizing salts.