SAF 2507®

BarDatablad

Datablad opdateret 2021-10-07 11:08 (afløser alle tidligere versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

SAF 2507® is a high alloy duplex (austenitic-ferritic) stainless steel for service in highly corrosive conditions. The grade is characterized by:

  • Excellent resistance to stress corrosion cracking in chloride-bearing environments
  • Excellent resistance to pitting and crevice corrosion
  • High resistance to general corrosion
  • Very high mechanical strength
  • Physical properties that offer design advantages
  • High resistance to erosion corrosion and corrosion fatigue good weldability
  • Excellent mechanical properties that allow for lighter constructions, more compact design and less welding

Standards

  • : S32750
  • : 1.4410
  • : X2CrNiMoN25-7-4

Product standards

  • EN 10088-3, (dimensions up to 160 mm)
  • EN 10272, EN 10222-5
  • ASTM A479, ASTM A276
  • NORSOK MDS D57 Rev 4, Rev 5
  • Suitable for manufacturing of components in accordance with ASTM A182

Approvals

  • Pressure Equipment Directive (2014/68/EU)
  • NORSOK M650 Ed. 4, NORSOK M630 Ed. 6, dimensions up to 250 mm.
  • DNV, dimensions up to 250 mm
  • Pre-approval for PMA

Certificate

Status according to EN 10 204/3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.