Sandvik 12C27™

BilletsDatablad

Datablad opdateret 2019-11-12 12:06 (afløser alle tidligere versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 12C27™ is a martensitic stainless chromium steel.
After heat treatment the composition of carbon and chromium gives a unique combination of properties including:

  • Very high hardness
  • Good corrosion resistance
  • Very high wear resistance

Standards

  • : 420
  • : S42000

Certificates

Status according to EN 10 204 3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.