Sandvik 5R60

BilletsDatablad

Datablad opdateret 2020-12-10 06:47 (afløser alle tidligere versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 5R60 is a molybdenum-alloyed (min 2.5%) austenitic stainless chromium-nickel steel and a controlled carbon content in order to obtain improved strength at high temperatures.

Standards

  • : 316, 316H
  • : S31600, S31609
  • : 1.4436
  • : 1.4436
  • : 2343
  • : Z7CND 18-14-03
  • : 316S11

Product standard

  • EN 10088-3
  • ASTM A-314

Suitable for production of flanges etc. acc. to ASTM A-182

Certificates

Status according to EN 10 204 3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via e-mail