Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Aminide is a Polyamide-imide insulation. It has excellent thermal endurance, solvent resistance.

Typical applications are within fractional and integral horse power motors (hermetic and open), automotive and hand tool armatures, dry type transformers.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.