Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sulfone polymers are high-heat plastics with a clear advantage. These amorphous thermoplastics offer more toughness, strength and hydrolytic stability than many other transparent plastics. They withstand prolonged exposure to water, chemicals and temperatures – handling a broad range of end-use temperatures from -40°C to 204°C (-40°F to 400°F).

We have developed proprietary processing techniques to allow the application of these materials on our alloy offerings; they can be applied at thicknesses as thin as 2.5 microns. Sulfones are traditionally applied using extrusion or injection molding, and application of thicknesses below 1 mil are atypical of these processing methods. In-house processing capability of these resins has also been developed, allowing very thin layers of polymer to be applied, yet still retaining the polymer’s unique characteristics.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.