Sandvik 10C16Mo3V1

Strip steelDatablad

Datablad opdateret 2021-09-23 06:12 (afløser alle tidligere versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 10C16Mo3V1 is an 8% chromium steel known for its good wear resistance properties and toughness. The grade is suitable for tools and knives in challenging applications, such as garden tools and harvest knives.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via e-mail