Sandvik 11R51

Strip steelDatablad

Datablad opdateret 2020-12-10 06:47 (afløser alle tidligere versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 11R51 is an austenitic stainless steel with excellent spring properties that in most cases fulfill demands regarding corrosion resistance, mechanical strength, fatigue and relaxation properties. Compared with the standard grade Sandvik 12R11, Sandvik 11R51 offers:

  • Higher tensile strength and tempering effect
  • Higher relaxation resistance, especially at elevated temperatures
  • Higher fatigue strength
  • Better corrosion resistance, due to the addition of molybdenum

Service temperature: up to 300°C (570°F)

Standards

  • : 1.4310
  • : X 10 CrNi 18-8
  • : 2331

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via e-mail