Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 13C is a hardened and tempered carbon precision strip steel. The characteristics of Sandvik 13C strip steel are:

  • Good etchability
  • Close dimensional tolerances
  • Good flatness
  • Good surface finish
  • Good wear resistance
  • Good shape after etching and subsequent fabrication
  • Good response to laser re-hardening

Standards

  • : (1.0612)
  • : CK 65

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.