Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 19C27 is a martensitic stainless chromium steel with high carbon content. After heat treatment the grade is characterized by:

  • Very high hardness
  • Very good wear resistance

Sandvik 19C27 is mainly used for industrial knives for cutting synthetic fibre, paper and plastic films.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.