Sandvik 20C for pad printing applications

Strip steelDatablad

Datablad opdateret 2020-08-27 12:07 (afløser alle tidligere versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 20C is a hardened and tempered carbon steel used for pad printing applications. The grade is characterized by:

  • Excellent surface finish
  • Good flatness
  • Good etchability
  • High strength and wear resistance
  • Low level of non-metallic inclusions
  • Good dimensional tolerances

Standards

  • : 1095
  • : 1.1274

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.