Sandvik 316LVM

Strip steelDatablad

Datablad opdateret 2021-09-23 06:06 (afløser alle tidligere versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 316LVM is a vacuum remelted, molybdenum alloyed, austenitic stainless steel and is used for implant and other medical applications. It is also suitable for the watch industry because of its absolute cleanliness and excellent polishing properties.

The grade is characterized by:

  • High strength
  • High fatigue strength
  • Excellent micro-cleanliness
  • Excellent structural homogeneity
  • High surface finish

Standards

  • : S31673
  • : 1.4441

Testing and certification can be performed according to ASTM F139 and ISO 5832-1.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.